023 9396 0313 Get a written quote

Split lead

Why does lead split on a roof?

The short answer

Lead splits when it is not free to move. Sheet expands and contracts as the temperature rises and falls, and lead that is fixed too tightly, laid in too long a run or cut too thin for its detail strains until it cracks, which can happen along a fold or at a fixing. Foot traffic, a sharp edge or movement in the structure below can also tear it. A patch over the split leaves the cause in place.

A crack across a lead sheet has a reason behind it. Why lead splits, what to look for and how a split is put right.

Split old lead flashing pulling away from a brick abutment

Why lead moves in the first place

Lead is a soft metal, and like other metals it grows a little as it warms and shrinks again as it cools, so even a small change in temperature moves the sheet. On a roof that happens every day and across every season, and a dark sheet in sun is warmer than the air around it. The change in any one hour is small, but it repeats for decades.

Good leadwork plans for it. Sheets are cut in separate lengths and joined with laps, rolls and drips, so that each piece can slide a little over the next, and fixings hold the top edge of a length while leaving the rest of it free. A detail laid that way carries its movement without strain, and the lap still sheds water downhill.

A split is what happens when that freedom has been taken away. The sheet cannot slide, so the stress finds the weakest line in it, which is often a bend or a nail hole, and the metal tears there. The crack is the sign of a cause, and the cause lies in the way the sheet was cut, nailed and supported as much as in the metal itself.

Causes a survey looks for

When we find a split, we look at how the sheet was laid before we look at the crack itself. These are the usual points:

  • A run that is too long for its thickness, so the movement over its length is more than the laps can take.
  • Fixings placed too low or too many, which pin the sheet so it cannot slide.
  • Lead cut too thin for the detail. Royston Lead's brochure lists code 3 for soakers only and codes 4 to 6 for flashings, so thin lead in a flashing is a mismatch.
  • Sharp bends and folds worked over and over, which weaken the metal at the crease.
  • Damage from a ladder, a boot or a tool, or from debris held against the sheet.
  • A structure that has moved, so that the lead is being pulled by the wall or the timber beneath it.

More than one of these can apply at once, and a survey says which seem to be in play on your roof. Our answer on what lead code is used for flashing sets out the codes.

What the position of a split can tell you

Where a crack sits is a clue to why it is there, and photographs help us read it before we go up. A few patterns are worth noting:

  • A crack along a fold or a roll can point to movement that could not be taken at that point.
  • A line of cracks along the nails suggests the sheet was fixed too tightly or too low.
  • A split near a lap or step may mean the lap is too short or the length above has crept down onto it.
  • Isolated tears and dents point to damage rather than to movement.

The same split appearing again in the same place after a repair means the cause has not been dealt with. That is worth telling the roofer, who can then look at how the sheet is held and not just at the crack, and it is why dated photographs of the first repair are useful.

Indoors, a split can show as a stain well away from the crack, since rain runs along the timber before it drops. The stain tells you a joint is open somewhere above, and the survey traces it back to the lead.

How a split is put right

The repair follows the cause. One short tear in otherwise healthy lead may be trimmed out and a new piece let in. Where the sheet has cracked in several places, or the run is simply too long, a fresh length goes down, cut in a code that suits the detail and fixed so that it can slide. A valley or a bay roof may need to be relaid in fresh lengths, once the boards beneath have been checked.

Mastic or tape over the split can hold a leak back briefly, but the strain stays where it was, and our answer on whether lead can be repaired with sealant explains why. Our guide to lead flashing repairs goes through the choices between patching, refixing and renewing.

When the survey is finished you get one written total for the work, and the quote says what is being replaced and why. If the split points to a laying fault, the quote says so, so you know what will be done differently this time. Our lead roofing page lists the other leadwork we carry out.

Related questions

Does a split in lead always mean the whole sheet must go?

No. A short split in sound lead may be cut out and a new piece fitted in its place. If the sheet is cracked in several places, or was laid with too long a run, new lengths make more sense. The survey tells you which applies to your roof.

Can I walk on lead to check for splits?

It is best not to. Foot traffic can tear or dent lead, and the roof edge is where a fall happens. HSE advises against assuming that any roof will carry a person. Use the zoom on a phone from the lawn or a bedroom window instead, and let a roofer inspect it.